Suche

 

ATALLOY

Iron based alloys made by atomization. The manufacturing process of our iron based alloys guarantees an even distribution of the components and prevents segregation

Advantages:

  • self-sharpening of the matrix
  • low oxygen content
  • usable for various diamond tool applications
  • can be used pure or as an additive

 

Material

Composition

Grain size(µm)

Sintering range (°C)

Hardness range (HRB)

Density range (g/cm³)

Apparent density(g/cm³)

ATALLOY-W1000

FeCu20

<45

820 - 940

~90

1500

3,3 - 3,7

ATALLOY-W2000

FeCu30

<45

780 - 940

>89

820

3,2 - 3,5

ATALLOY-W3000

FeCuSn5

<45

700 - 820

95 - 103

750

3,1 - 3,2

Sintering data is available upon request.